polymerization of aluminum use the method:

Solid product with water at room temperature 1:2.5-1:3 [weight ratio] mixed stirred for about 30 minutes. Drugs completely dissolved, add 30-40 times diluted with water or diluted into a liquid according to the desired concentration using the [the greater the source water turbidity, the secondary dilution add water to the more].
Source water turbidity in the 100-500mg / L, the dosage of 5-10mg per one thousand tons of water dosage is 5-10kg. Small scale water quality characteristics of the best pre-select the best value, and then vote with.
polymerization of aluminum packaging is lined with plastic bags, with outer surface of plastic laminating bags, each bag weighs 25 kilograms.
polymerization of aluminum stored in a cool, dry place to prevent the sun and rain.